描述
NORYL WM220A Resin is a 20% glass fiber reinforced blend of polyphenylene ether (PPE) and polystyrene (PS), manufactured by SABIC. This injection moldable grade exhibits excellent long-term hydrolytic stability, very low water absorption, and heat/hot water resistance.
The 20% glass reinforcement provides enhanced stiffness and strength while maintaining good dimensional stability and low warpage. This grade is an excellent candidate for various water management applications such as pump housings, impellers, and valves.
NORYL WM220A is part of the NORYL family of modified PPE resins, consisting of amorphous blends of PPO™ resin (polyphenylene ether) and polystyrene. These resins combine the inherent advantages of PPO—affordable high heat resistance, good electrical properties, outstanding hydrolytic stability, and the ability to use non-halogen flame retardant packages—with excellent dimensional stability, good processability, and low specific gravity. See NORYL FE1520PW resin for NSF/ANSI 61 and global potable water compliant versions.
Physical property data is determined using test methods established by ASTM International, the globally recognized standards organization.
For more NORYL grades and technical information, please visit our PPO/PPE product page.
Key Features of NORYL WM220A Resin
-
20% Glass Fiber Reinforced – Provides enhanced stiffness, strength, and dimensional stability
-
Excellent Long-Term Hydrolytic Stability – Resists degradation in wet environments; ideal for water contact applications
-
Very Low Water Absorption – 0.06% water absorption (24 hrs)
-
Heat/Hot Water Resistance – Maintains properties in elevated temperature water applications
-
High Stiffness – Flexural modulus of 5,640 MPa
-
High Heat Resistance – DTUL of 141°C at 1.82 MPa (6.4mm)
-
High Impact Strength – Notched Izod impact of 150 J/m (1/8 in)
-
Good Dimensional Stability – Low warpage and low shrinkage (0.2–0.4% flow, 3.2mm)
-
High Structural Strength – Flexural strength of 150 MPa
-
Excellent Processability – Melt flow index of 9.4 g/10min (300°C/5.0kg)
-
Non-Halogenated Options – Available in non-halogenated flame retardant grades
-
Good Chemical Resistance – Good resistance to many cleaning agents and acids
-
Creep Resistance – Maintains dimensional integrity under sustained load
-
Heat Stabilized – Maintains properties under thermal exposure
-
Amorphous / Low Warpage – Low shrinkage characteristics
-
Non UL Rated – Suitable for applications where flame retardancy is not a primary requirement
-
Injection Moldable – Suitable for standard injection molding processes
Typical Applications for NORYL WM220A Resin
| Industry | Typical Components & Considerations |
|---|---|
| Water Management | Pump housings, impellers – excellent long-term hydrolytic stability, heat/hot water resistance, high stiffness |
| Water Management | Valves – very low water absorption, good dimensional stability, creep resistance |
| Building & Construction | Building components, water management systems – hydrolytic stability, dimensional stability |
| Industrial | Fluid handling equipment – chemical resistance, high structural strength |
Typical Properties of NORYL WM220A Resin
| Property | Value | Test Method |
|---|---|---|
| Physical | ||
| Density | 1,230 kg/m³ (1.23 g/cm³) | ASTM D792 |
| Water Absorption (24 hrs) | 0.06% | ASTM D570 |
| Mold Shrinkage, Flow (3.2mm) | 0.2 – 0.4% | ASTM D955 |
| Melt Flow Index (MFI) (300°C/5.0kg) | 9.4 g/10min | ASTM D1238 |
| Mechanical | ||
| Flexural Modulus | 5,640 MPa | ASTM D790 |
| Flexural Strength | 150 MPa | ASTM D790 |
| Rockwell Hardness | R 124 | ASTM D785 |
| Izod Impact, Notched (1/8 in) | 150 J/m | ASTM D256 |
| Thermal | ||
| DTUL @ 1.82 MPa (264 psi, 6.4mm) | 141°C | ASTM D648 |
| Electrical | ||
| Surface Resistivity | 1×10¹⁶ Ω | ASTM D257 |
| Processing | ||
| Processing Method | Injection molding | — |
| Certifications | ||
| Food Contact | NSF 51 | — |
| Drinking Water Contact | NSF 61 | — |
Important Notes on Typical Data:
Values listed are typical and sourced from manufacturer data sheets. They do not constitute binding product specification.
Batch-to-batch deviations may exist. For critical applications, validate performance with batch-specific COA certificate.
Final performance depends on processing conditions and part design.
Manufacturer official TDS shall serve as definitive technical reference. Request the latest official TDS from our sales team.
Processing Guidelines for NORYL WM220A Resin
| Step | Process |
|---|---|
| Processing Method | Injection molding |
| Drying Temperature | Refer to full TDS |
| Drying Time | Refer to full TDS |
| Melt Temperature | Refer to full TDS |
| Mold Temperature | Refer to full TDS |
| Storage | Store in original, sealed packaging in a cool, dry place away from direct sunlight |
Critical Processing Warnings:
Injection Molding: NORYL WM220A is specifically designed for injection molding.
Drying: Proper drying is critical to prevent hydrolysis and achieve optimal mechanical properties. Refer to the full TDS for specific drying conditions.
Glass Reinforcement: This grade contains 20% glass fiber, which may require processing adjustments for optimal surface finish and fiber orientation.
Non UL Rated: This grade is Non UL Rated. Material selection should be driven by thermal, mechanical, and performance requirements rather than flame classification standards.
Certifications: This grade carries NSF 51 (food contact) and NSF 61 (drinking water contact) certifications. Ensure processing conditions maintain compliance. See NORYL FE1520PW resin for NSF/ANSI 61 and global potable water compliant versions.
Storage: Store in original, sealed packaging in a cool, dry place away from direct sunlight.
Related Products for NORYL WM220A Resin
Explore Engineering Plastics – Browse all engineering plastic materials
About Our Company – Learn more about our supply capabilities and quality assurance
Technical Documents for NORYL WM220A Resin
| Document Type | Description & Source |
|---|---|
| Manufacturer Official TDS | Complete physical, thermal, and mechanical properties of NORYL WM220A |
| Manufacturer Official SDS | GHS-compliant safety documentation |
| COA (Certificate of Analysis) | Batch-specific quality certification |
| NSF 51 / NSF 61 Certifications | Food contact and drinking water contact compliance |
Request any document above by:
Email: ruiqingchem@gmail.com
Online form: Our contact page
We reply within one working business day. Please clearly state product (NORYL WM220A) and document type you require.
FAQ about NORYL WM220A Resin
Q1: What is NORYL WM220A?
A: NORYL WM220A Resin is a 20% glass fiber reinforced blend of polyphenylene ether (PPE) and polystyrene (PS) from SABIC. It is an injection moldable grade exhibiting excellent long-term hydrolytic stability, very low water absorption, and heat/hot water resistance.
Q2: What are the key features of NORYL WM220A?
A: 20% glass reinforcement, excellent long-term hydrolytic stability, very low water absorption (0.06% water absorption), high heat resistance (DTUL 141°C at 1.82 MPa), high stiffness (flexural modulus 5,640 MPa), high impact strength (150 J/m notched Izod), good dimensional stability (0.2–0.4% shrinkage), NSF 51 and NSF 61 certified, and excellent processability.
Q3: What are the typical applications for NORYL WM220A?
A: Water management applications including pump housings, impellers, valves, building components, and fluid handling equipment requiring long-term hydrolytic stability and heat/hot water resistance.
Q4: Is NORYL WM220A NSF certified for potable water?
A: Yes, NORYL WM220A carries NSF 61 certification for drinking water contact. For NSF/ANSI 61 and global potable water compliant versions, see NORYL FE1520PW resin.
Q5: What is the recommended processing method for NORYL WM220A?
A: Injection molding. Refer to the full TDS for specific drying, melt, and mold temperature conditions.
Q6: What is the flexural modulus of NORYL WM220A?
A: The flexural modulus is 5,640 MPa.
Q7: Is NORYL WM220A UL rated?
A: No, NORYL WM220A is Non UL Rated. Material selection should be driven by thermal, mechanical, and performance requirements rather than flame classification standards.
Q8: What is the melt flow index of NORYL WM220A?
A: The melt flow index (MFI) is 9.4 g/10min at 300°C/5.0kg.
Q9: What is the heat deflection temperature of NORYL WM220A?
A: The DTUL at 1.82 MPa (264 psi, 6.4mm, unannealed) is 141°C.
Q10: What regions is NORYL WM220A available in?
A: Asia Pacific.
CTA (Call to Action)
Ready to order NORYL WM220A?
To get a precise quotation and professional technical support, please share:
-
Required quantity (kg)
-
Destination port or delivery address
-
Target application (pump housings, impellers, valves, water management, etc.)
-
Document requirement (TDS, SDS, COA, NSF docs, etc.)
Sample Policy:
-
Samples are for laboratory validation tests only, not for production use.
-
Buyer bears international sample-shipping freight.
-
If bulk-product performance deviates from sample reference, manufacturer official TDS serves as the authoritative benchmark.
Take action now:
-
📧 Email Us – ruiqingchem@gmail.com
-
📝 Send Inquiry – Use our quick inquiry form
-
💬 Live Chat – Click the bottom-right chat widget to speak directly with our team
After-Sales Support
| Service | Details |
|---|---|
| Quality Inspection Period | All quality-related claims must be submitted within 7 working days after delivery, supported by test data and photographic evidence. |
| Return / Exchange Policy | Confirmed product defects caused by our side trigger replacement or refund. Terms and conditions apply. |
| Logistics Damage | Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim-document preparation. |
| Technical Support | Remote technical guidance available. On-site troubleshooting can be arranged upon special request. |
| Export Documentation | We supply commercial invoice, packing list, bill of lading, COA, and additional compliance certificates on request. |
Disclaimer
DISCLAIMER: All technical data is referenced from original manufacturer typical values for NORYL WM220A. Our company acts as authorized distributor/trader rather than original manufacturer. Final performance depends on processing conditions and part design. Buyers shall independently validate product suitability for individual applications. Our firm bears no liability for product failure caused by improper processing or improper usage. Always reference the latest manufacturer official TDS of NORYL WM220A as the definitive specification.