NORYL PN235 – Non-Reinforced PPE/HIPS Blend for Plated Automotive Applications

基础信息

品名
NORYL PN235 Resin
牌号
PN235
厂商
SABIC (Saudi Basic Industries Corporation)
材料类型
PPE/PPO-Based Alloy (Polyphenylene Ether/Polyphenylene Oxide)
产品形态
Pellets – Injection Molding
特点
Non-reinforced; good impact resistance (347 J/m notched Izod); low moisture absorption; creep resistance; dimensional stability; hydrolytic stability; platable; CTI >600V; amorphous; low shrinkage; low specific gravity; No PFAS intentionally added; RoHS compliant

描述

NORYL PN235 Resin is a non-reinforced blend of polyphenylene ether (PPE) and high impact polystyrene (HIPS), manufactured by SABIC. This compression and injection moldable grade exhibits good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability.

NORYL PN235 is specifically designed for platable applications, making it an excellent candidate for a variety of plated automotive exterior components. The material is formulated to accept electroplating finishes, providing both aesthetic appeal and functional performance. This product does not contain PFAS intentionally added during the manufacturing process. Physical property data is determined using test methods established by ASTM International, the globally recognized standards organization.

For more NORYL grades and technical information, please visit our PPO/PPE product page.

Key Features of NORYL PN235 Resin

  • Platable – Designed to accept electroplating finishes for automotive exterior applications 

  • Non-Reinforced PPE/HIPS Blend – Unfilled formulation for balanced performance

  • Good Impact Resistance – Notched Izod impact of 347 J/m at 23°C 

  • Low Moisture Absorption – Maintains properties in humid environments

  • Creep Resistance – Maintains dimensional integrity under sustained load

  • Dimensional Stability – Precise part geometry with low warpage

  • Hydrolytic Stability – Resists degradation in wet environments 

  • CTI >600V – Excellent comparative tracking index for electrical applications 

  • Amorphous / Low Shrinkage – Low shrinkage characteristics

  • Low Specific Gravity – Lightweight for automotive applications

  • No PFAS Intentionally Added – Compliant with environmental regulations 

  • Compression & Injection Moldable – Suitable for both compression and injection molding 

Typical Applications for NORYL PN235 Resin

Industry Typical Components & Considerations
Automotive Exteriors Plated exterior components, chrome-plated automotive parts – platable, good impact resistance, dimensional stability 
Automotive Plated decorative and functional automotive components
Injection Molding Various injection molded plated parts 
Compression Molding Compression molded plated components

Typical Properties of NORYL PN235 Resin

Property Value Test Method
Physical
Density / Specific Gravity 1,050 kg/m³ (1.05 g/cm³) ASTM D792 
Linear Mold Shrinkage, Flow 0.50 – 0.70% SABIC Method 
Mechanical
Tensile Stress, Yield (Type I, 50 mm/min) 37 MPa ASTM D638 
Tensile Strain, Break (Type I, 50 mm/min) 72% ASTM D638 
Flexural Stress, Yield (2.6 mm/min, 100 mm span) 55 MPa ASTM D790 
Flexural Modulus (2.6 mm/min, 100 mm span) 1,820 MPa ASTM D790 
Impact
Izod Impact, Notched (23°C, 1/8 in) 347 J/m ASTM D256 
Izod Impact, Notched (-40°C, 1/8 in) 133 J/m ASTM D256 
Thermal
HDT, 0.45 MPa (66 psi, 6.4mm, unannealed) 112°C ASTM D648 
HDT, 1.82 MPa (264 psi, 6.4mm, unannealed) 104°C ASTM D648 
CTE, Flow (0°C to 100°C) 7.56E-05 1/°C ASTM E831 
Electrical
Arc Resistance 60 – 119 s (Tungsten) ASTM D495 
Comparative Tracking Index (CTI) >600 V UL 746A 
High Amp Arc Ignition (HAI) 30 – 59 (Surface) UL 746A 
Flammability
Flame Rating (1.5mm) HB IEC 60695-11-10 
Processing
Drying Temperature 95 – 105°C
Drying Time 3 – 4 hours
Maximum Moisture Content ≤ 0.02%
Nozzle Temperature 265 – 295°C
Rear Zone 1 Temperature 230 – 280°C
Middle Zone 2 Temperature 245 – 290°C
Front Zone 3 Temperature 255 – 295°C
Melt Temperature 265 – 295°C
Mold Temperature 65 – 95°C
Back Pressure 0.3 – 0.7 MPa
Screw Speed 20 – 100 rpm
Vent Depth 0.038 – 0.051 mm

Important Notes on Typical Data:

Values listed are typical and sourced from manufacturer data sheets. They do not constitute binding product specification.

Batch-to-batch deviations may exist. For critical applications, validate performance with batch-specific COA certificate.

Final performance depends on processing conditions and part design.

Manufacturer official TDS shall serve as definitive technical reference. Request the latest official TDS from our sales team.

Processing Guidelines for NORYL PN235 Resin

Step Process
Processing Methods Injection molding, compression molding 
Drying Temperature 95 – 105°C 
Drying Time 3 – 4 hours 
Maximum Moisture Content ≤ 0.02% 
Rear – Zone 1 Temperature 230 – 280°C 
Middle – Zone 2 Temperature 245 – 290°C 
Front – Zone 3 Temperature 255 – 295°C 
Nozzle Temperature 265 – 295°C 
Melt Temperature 265 – 295°C 
Mold Temperature 65 – 95°C 
Back Pressure 0.3 – 0.7 MPa 
Screw Speed 20 – 100 rpm 
Vent Depth 0.038 – 0.051 mm 
Storage Store in original, sealed packaging in a cool, dry place away from direct sunlight

Critical Processing Warnings:

Injection & Compression Molding: NORYL PN235 is suitable for both injection molding and compression molding processes .

Drying: Proper drying is critical to prevent hydrolysis and achieve optimal mechanical properties. Dry at 95–105°C for 3–4 hours .

Platable Design: This grade is specifically formulated for plating applications. Ensure proper processing conditions to achieve optimal plating adhesion and surface finish.

Storage: Store in original, sealed packaging in a cool, dry place away from direct sunlight.

Related Products

Explore Engineering Plastics – Browse all engineering plastic materials

About Our Company – Learn more about our supply capabilities and quality assurance

Technical Documents for NORYL PN235 Resin

Document Type Description & Source
Manufacturer Official TDS Complete physical, thermal, and mechanical properties of NORYL PN235
Manufacturer Official SDS GHS-compliant safety documentation
COA (Certificate of Analysis) Batch-specific quality certification
UL Yellow Card UL safety certification

Request any document above by:

Email: ruiqingchem@gmail.com

Online form: Our contact page

We reply within one working business day. Please clearly state product (NORYL PN235) and document type you require.

FAQ about NORYL PN235 Resin

Q1: What is NORYL PN235?

A: NORYL PN235 is a non-reinforced blend of polyphenylene ether (PPE) and high impact polystyrene (HIPS) from SABIC . It is a compression and injection moldable grade with good impact resistance, low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability .

Q2: What are the key features of NORYL PN235?

A: It offers good impact resistance (347 J/m notched Izod), low moisture absorption, creep resistance, dimensional stability, hydrolytic stability, plateability, CTI >600V, low specific gravity, amorphous/low shrinkage characteristics, and No PFAS intentionally added .

Q3: What are the typical applications for NORYL PN235?

A: Typical applications include plated automotive exterior components, chrome-plated automotive parts, and various plated decorative and functional automotive components .

Q4: Can NORYL PN235 be plated?

A: Yes, NORYL PN235 is specifically designed for platable applications, making it an excellent candidate for electroplating finishes on automotive exterior components .

Q5: What is the CTI rating of NORYL PN235?

A: The Comparative Tracking Index (CTI) is >600V, indicating excellent tracking resistance for electrical applications .

Q6: What is the recommended processing method for NORYL PN235?

A: NORYL PN235 is suitable for injection molding and compression molding .

Q7: What is the recommended drying condition for NORYL PN235?

A: Dry at 95 – 105°C for 3 – 4 hours prior to processing .

Q8: What is the recommended melt temperature for NORYL PN235?

A: 265 – 295°C.

Q9: What is the specific gravity of NORYL PN235?

A: The specific gravity is 1.05 g/cm³ (1,050 kg/m³) .

Q10: Is NORYL PN235 UL rated?

A: NORYL PN235 carries a UL94 flame rating of HB at 1.5mm thickness.

Q11: What regions is NORYL PN235 available in?

A: It is available in the Americas (North America, South and Central America) and Asia / Pacific .

Q12: What is the lead time for orders?

A: Regular orders ship within 7-10 working days after payment confirmation. Large-volume orders can be negotiated separately.

CTA (Call to Action)

Ready to order NORYL PN235?

To get a precise quotation and professional technical support, please share:

  • Required quantity (kg)

  • Destination port or delivery address

  • Target application (plated automotive exteriors, automotive components, etc.)

  • Document requirement (TDS, SDS, COA, UL docs, etc.)

Sample Policy:

  • Samples are for laboratory validation tests only, not for production use.

  • Buyer bears international sample-shipping freight.

  • If bulk-product performance deviates from sample reference, manufacturer official TDS serves as the authoritative benchmark.

Take action now:

  • 📧 Email Us – ruiqingchem@gmail.com

  • 📝 Send Inquiry – Use our quick inquiry form

  • 💬 Live Chat – Click the bottom-right chat widget to speak directly with our team

After-Sales Support

Service Details
Quality Inspection Period All quality-related claims must be submitted within 7 working days after delivery, supported by test data and photographic evidence.
Return / Exchange Policy Confirmed product defects caused by our side trigger replacement or refund. Terms and conditions apply.
Logistics Damage Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim-document preparation.
Technical Support Remote technical guidance available. On-site troubleshooting can be arranged upon special request.
Export Documentation We supply commercial invoice, packing list, bill of lading, COA, and additional compliance certificates on request.

Disclaimer

DISCLAIMER: All technical data is referenced from original manufacturer typical values for NORYL PN235. Our company acts as authorized distributor/trader rather than original manufacturer. Final performance depends on processing conditions and part design. Buyers shall independently validate product suitability for individual applications. Our firm bears no liability for product failure caused by improper processing or improper usage. Always reference the latest manufacturer official TDS of NORYL PN235 as the definitive specification.

Technical Documents

Download technical data sheets, safety data sheets and certificates for this material.

TDS Files

Technical document available for review or download.

0 Files
No TDS file uploaded yet.

MSDS Files

Technical document available for review or download.

0 Files
No MSDS file uploaded yet.