描述
NORYL NC208 Resin is an 8% carbon fiber reinforced blend of polyphenylene ether (PPE) and polystyrene (PS), manufactured by SABIC. This injection moldable grade is specifically designed for conductive/ESD-safe applications requiring electrostatic discharge protection. It contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V-1 at 1.5mm.
NORYL NC208 Resin exhibits high stiffness, good dimensional stability, hydrolytic stability, and very low moisture absorption (0.06%). The carbon fiber reinforcement provides surface resistivity in the range of 1×10⁹ to 1×10¹² Ω, making it suitable for applications where static control is critical. This material is an excellent candidate for electronic components, connectors, trays, carriers, and drone components requiring ESD protection. This product does not contain PFAS intentionally added during the manufacturing process.
For more NORYL grades and technical information, please visit our PPO/PPE product page.
Key Features of NORYL NC208 Resin
-
8% Carbon Fiber Reinforced – Provides enhanced stiffness and electrical conductivity
-
ESD Safe / Conductive – Surface resistivity of 1×10⁹ to 1×10¹² Ω for electrostatic discharge protection
-
Halogen-Free Flame Retardant – Non-brominated, non-chlorinated flame retardant system
-
UL94 V-1 Rated – V-1 at 1.5mm thickness
-
High Stiffness – Flexural modulus of 4,900 MPa
-
Good Dimensional Stability – Precise part geometry with low warpage
-
Very Low Moisture Absorption – 0.06% water absorption (23°C/24hrs)
-
Hydrolytic Stability – Resists degradation in wet environments
-
Good Surface Quality – Carbon fiber filled with good surface appearance
-
Low Warpage – Minimizes deformation during processing and use
-
Non-Reinforced PPE/PS Blend – Unfilled formulation for balanced performance
-
No PFAS Intentionally Added – Compliant with environmental regulations
-
Injection Moldable – Suitable for standard injection molding processes
-
RoHS Compliant – Meets global environmental standards
Typical Applications for NORYL NC208 Resin
| Industry | Typical Components & Considerations |
|---|---|
| Electrical & Electronics | ESD-safe electronic components, connectors – surface resistivity 1E9–1E12 Ω, UL94 V-1, dimensional stability |
| Component Handling | Trays and carriers for electronics – static dissipation, low warpage |
| Industrial | ESD-safe industrial components – conductivity, stiffness |
| Drones & UAVs | Drone components – lightweight, ESD protection, dimensional stability |
| Automotive | Automotive electronic components – ESD protection, heat resistance |
Typical Properties of NORYL NC208 Resin
| Property | Value | Test Method |
|---|---|---|
| Physical | ||
| Density / Specific Gravity | 1.14 g/cm³ (1140 kg/m³) | ASTM D792 |
| Water Absorption (23°C/24hrs) | 0.06% | ASTM D570 |
| Linear Mold Shrinkage, Flow (3.2mm) | 0.2 – 0.4% | SABIC Method |
| Mold Shrinkage, X-Flow (3.2mm) | 0.3 – 0.5% | SABIC Method |
| Melt Flow Rate (300°C/5.0kg) | 30 g/10min | ASTM D1238 |
| Melt Volume Rate (300°C/5.0kg) | 25 cm³/10min | ISO 1133 |
| Mechanical (ASTM) | ||
| Tensile Modulus | 4,500 – 5,000 MPa | ASTM D638 |
| Tensile Strength, Break | 70 MPa | ASTM D638 |
| Tensile Strain, Break | 2.1% | ASTM D638 |
| Flexural Modulus | 4,900 MPa | ASTM D790 |
| Flexural Strength | 117 MPa | ASTM D790 |
| Mechanical (ISO) | ||
| Tensile Modulus | 4,640 – 6,140 MPa | ISO 527 |
| Tensile Stress, Break | 68 – 74 MPa | ISO 527 |
| Tensile Strain, Break | 1.9 – 2.5% | ISO 527 |
| Flexural Modulus | 4,500 – 5,800 MPa | ISO 178 |
| Flexural Strength | 105 – 125 MPa | ISO 178 |
| Impact | ||
| Izod Impact, Notched (23°C) | 58 J/m | ASTM D256 |
| Charpy Notched Impact (23°C) | 6 kJ/m² | ISO 179/1eA |
| Thermal | ||
| HDT, 1.82 MPa (3.2mm, unannealed) | 132°C | ASTM D648 |
| HDT, 0.45 MPa (3.2mm, unannealed) | 140°C | ASTM D648 |
| CTE, Flow (-30°C to 30°C) | 2.5E-05 – 4.0E-05 1/°C | TMA |
| Electrical | ||
| Surface Resistivity | 1E9 – 1E12 Ω | ASTM D257 |
| Flammability | ||
| Flame Rating (1.5mm) | V-1 | UL 94 |
| UL Yellow Card | E207780-228564 | UL |
Important Notes on Typical Data:
Values listed are typical and sourced from manufacturer data sheets. They do not constitute binding product specification.
Batch-to-batch deviations may exist. For critical applications, validate performance with batch-specific COA certificate.
Final performance depends on processing conditions and part design.
Manufacturer official TDS shall serve as definitive technical reference. Request the latest official TDS from our sales team.
Processing Guidelines for NORYL NC208 Resin
| Step | Process |
|---|---|
| Drying Temperature | 100 – 120°C |
| Drying Time | 3 – 5 hours |
| Maximum Moisture Content | < 0.02% |
| Rear – Zone 1 Temperature | 240 – 280°C |
| Middle – Zone 2 Temperature | 250 – 290°C |
| Front – Zone 3 Temperature | 270 – 310°C |
| Nozzle Temperature | 270 – 310°C |
| Melt Temperature | 270 – 310°C |
| Mold Temperature | 70 – 110°C |
| Back Pressure | 0.5 – 1.0 MPa |
| Screw Speed | 40 – 80 rpm |
| Process | Injection Molding |
| Storage | Store in original, sealed packaging in a cool, dry place away from direct sunlight |
Critical Processing Warnings:
Injection Molding: NORYL NC208 is specifically designed for injection molding.
Drying: Proper drying is critical to prevent hydrolysis and achieve optimal mechanical properties. Dry at 100–120°C for 3–5 hours.
Carbon Fiber Reinforcement: This grade contains 8% carbon fiber, which may require processing adjustments for optimal surface finish and fiber orientation.
UL Compliance: This grade carries a UL94 V-1 rating at 1.5mm thickness. Ensure processing conditions maintain compliance.
Storage: Store in original, sealed packaging in a cool, dry place away from direct sunlight.
Related Products
Explore Engineering Plastics – Browse all engineering plastic materials
About Our Company – Learn more about our supply capabilities and quality assurance
Technical Documents for NORYL NC208 Resin
| Document Type | Description & Source |
|---|---|
| Manufacturer Official TDS | Complete physical, thermal, and electrical properties of NORYL NC208 |
| Manufacturer Official SDS | GHS-compliant safety documentation |
| COA (Certificate of Analysis) | Batch-specific quality certification |
| UL Yellow Card | E207780-228564 – UL safety certification |
Request any document above by:
Email: ruiqingchem@gmail.com
Online form: Our contact page
We reply within one working business day. Please clearly state product (NORYL NC208) and document type you require.
FAQ about NORYL NC208 Resin
Q1: What is NORYL NC208?
A: NORYL NC208 is an 8% carbon fiber reinforced blend of polyphenylene ether (PPE) and polystyrene (PS) from SABIC. It is an injection moldable grade with non-halogenated flame retardancy, UL94 V-1 rating, surface resistivity of 1E9–1E12 Ω, high stiffness, dimensional stability, and very low moisture absorption.
Q2: What are the key features of NORYL NC208?
A: It offers 8% carbon fiber reinforcement, ESD-safe conductivity (surface resistivity 1E9–1E12 Ω), halogen-free flame retardancy (UL94 V-1), high stiffness (flexural modulus 4,900 MPa), good dimensional stability, very low moisture absorption (0.06%), hydrolytic stability, low warpage, and RoHS compliance.
Q3: What are the typical applications for NORYL NC208?
A: Typical applications include ESD-safe electronic components, connectors, trays and carriers for electronics, industrial ESD-safe components, drone components, and automotive electronic components.
Q4: What is the surface resistivity of NORYL NC208?
A: The surface resistivity is 1×10⁹ to 1×10¹² Ω per ASTM D257.
Q5: What is the flame rating of NORYL NC208?
A: UL94 V-1 at 1.5mm thickness.
Q6: Is NORYL NC208 halogen-free?
A: Yes, it contains non-brominated, non-chlorinated flame retardant.
Q7: What is the recommended processing method for NORYL NC208?
A: NORYL NC208 is designed for injection molding.
Q8: What is the recommended drying condition for NORYL NC208?
A: Dry at 100 – 120°C for 3 – 5 hours prior to processing.
Q9: What is the recommended melt temperature for NORYL NC208?
A: 270 – 310°C.
Q10: What is the UL Yellow Card number for NORYL NC208?
A: E207780-228564.
Q11: What regions is NORYL NC208 available in?
A: Americas, Asia / Pacific, and Europe.
Q12: What is the lead time for orders?
A: Regular orders ship within 7-10 working days after payment confirmation. Large-volume orders can be negotiated separately.
CTA (Call to Action)
Ready to order NORYL NC208?
To get a precise quotation and professional technical support, please share:
-
Required quantity (kg)
-
Destination port or delivery address
-
Target application (ESD-safe electronics, connectors, trays, drones, etc.)
-
Document requirement (TDS, SDS, COA, UL docs, etc.)
Sample Policy:
-
Samples are for laboratory validation tests only, not for production use.
-
Buyer bears international sample-shipping freight.
-
If bulk-product performance deviates from sample reference, manufacturer official TDS serves as the authoritative benchmark.
Take action now:
-
📧 Email Us – ruiqingchem@gmail.com
-
📝 Send Inquiry – Use our quick inquiry form
-
💬 Live Chat – Click the bottom-right chat widget to speak directly with our team
After-Sales Support
| Service | Details |
|---|---|
| Quality Inspection Period | All quality-related claims must be submitted within 7 working days after delivery, supported by test data and photographic evidence. |
| Return / Exchange Policy | Confirmed product defects caused by our side trigger replacement or refund. Terms and conditions apply. |
| Logistics Damage | Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim-document preparation. |
| Technical Support | Remote technical guidance available. On-site troubleshooting can be arranged upon special request. |
| Export Documentation | We supply commercial invoice, packing list, bill of lading, COA, and additional compliance certificates on request. |
Disclaimer
DISCLAIMER: All technical data is referenced from original manufacturer typical values for NORYL NC208. Our company acts as authorized distributor/trader rather than original manufacturer. Final performance depends on processing conditions and part design. Buyers shall independently validate product suitability for individual applications. Our firm bears no liability for product failure caused by improper processing or improper usage. Always reference the latest manufacturer official TDS of NORYL NC208 as the definitive specification.