NORYL PPO534 Resin is a non-reinforced blend of polyphenylene ether (PPE) and polystyrene (PS), manufactured by SABIC. This high heat injection moldable grade exhibits high impact strength, dimensional stability, hydrolytic stability, and very low moisture absorption.
NORYL PPO534 is an excellent candidate for compounding applications. This product does not contain PFAS intentionally added during the manufacturing process. The material carries a UL94 flame rating of V-1 at 1.5mm.
For more NORYL grades and technical information, please visit our PPO/PPE product page.
Key Features of NORYL PPO534 Resin
-
Non-Reinforced PPE/PS Blend – Unfilled formulation for balanced performance and predictable processing
-
High Heat Resistance – Deflection temperature of 160°C at 1.82 MPa (264 psi)
-
High Impact Strength – Notched Izod impact of 137 J/m at 23°C
-
Dimensional Stability – Precise part geometry with low warpage
-
Hydrolytic Stability – Resists degradation in wet environments
-
Very Low Moisture Absorption – 0.03% water absorption (23°C/24hrs)
-
High Stiffness – Flexural modulus of 2,590 MPa
-
Good Strength – Tensile stress (yield) of 72 MPa
-
Excellent Electrical Properties – Surface resistivity of 1.00E+16 Ω
-
UL94 V-1 Rated – V-1 at 1.5mm thickness
-
RoHS Compliant – Meets global environmental standards
-
No PFAS Intentionally Added – Compliant with environmental regulations
-
Injection Moldable – Suitable for standard injection molding processes
Typical Applications for NORYL PPO534 Resin
| Industry | Typical Components & Considerations |
|---|---|
| Compounding | Resin blending, masterbatch production – excellent compatibility and processability |
| Material Handling | Material handling equipment and components |
| Drones | Drone components – dimensional stability, high impact resistance |
| Electrical & Electronics | Electrical components and housings – UL94 V-1, high heat resistance |
| Consumer Electronics | Mobile phones, computers, tablets – dimensional stability, hydrolytic stability |
| Injection Molding | Various injection molded components – high impact strength, dimensional stability |
Typical Properties of NORYL PPO534 Resin
| Property | Value | Test Method |
|---|---|---|
| Physical | ||
| Density / Specific Gravity | 1.08 g/cm³ (1,080 kg/m³) | ASTM D792 |
| Water Absorption (23°C/24hrs) | 0.03% | ASTM D570 |
| Mold Shrinkage, Flow (3.2mm) | 0.6 – 0.8% | SABIC Method |
| Mechanical | ||
| Tensile Stress, Yield | 72 MPa | SABIC – Japan Method |
| Tensile Strain, Break | 55% | SABIC – Japan Method |
| Flexural Stress | 104 MPa | ASTM D790 |
| Flexural Modulus | 2,590 MPa | ASTM D790 |
| Hardness, Rockwell R | 123 | ASTM D785 |
| Impact | ||
| Izod Impact, Notched (23°C) | 137 J/m | ASTM D256 |
| Thermal | ||
| Heat Deflection Temp (1.82 MPa, 6.4mm) | 160°C | ASTM D648 |
| Coefficient of Thermal Expansion (-30°C to 30°C) | 5.1E-05 1/°C | TMA |
| Electrical | ||
| Surface Resistivity | 1.00E+16 Ω | ASTM D257 |
| Relative Permittivity (50/60 Hz) | 2.58 | ASTM D150 |
| Flammability | ||
| Flame Rating (1.5mm) | V-1 | UL 94 |
| UL Yellow Card | Available | E45587 |
Important Notes on Typical Data:
Values listed are typical and sourced from manufacturer data sheets. They do not constitute binding product specification.
Batch-to-batch deviations may exist. For critical applications, validate performance with batch-specific COA certificate.
Final performance depends on processing conditions and part design.
Manufacturer official TDS shall serve as definitive technical reference. Request the latest official TDS from our sales team.
Processing Guidelines for NORYL PPO534 Resin
| Step | Process |
|---|---|
| Drying Temperature | 100 – 120°C |
| Drying Time | 3 – 4 hours |
| Maximum Moisture Content | < 0.02% |
| Rear – Zone 1 Temperature | 260 – 280°C |
| Middle – Zone 2 Temperature | 270 – 300°C |
| Front – Zone 3 Temperature | 290 – 320°C |
| Nozzle Temperature | 280 – 310°C |
| Melt Temperature | 290 – 320°C |
| Mold Temperature | 80 – 120°C |
| Back Pressure | 0.5 – 1.2 MPa |
| Screw Speed | 40 – 60 rpm |
| Process | Injection Molding |
| Storage | Store in original, sealed packaging in a cool, dry place away from direct sunlight |
Critical Processing Warnings:
Injection Molding: NORYL PPO534 is specifically designed for injection molding.
Drying: Proper drying is critical to prevent hydrolysis and achieve optimal mechanical properties. Dry at 100–120°C for 3–4 hours.
Mold Shrinkage: Measurements made from laboratory test coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design.
UL Compliance: This grade carries a UL94 V-1 rating at 1.5mm thickness. Ensure processing conditions maintain compliance.
Storage: Store in original, sealed packaging in a cool, dry place away from direct sunlight.
Related Products
Explore Engineering Plastics – Browse all engineering plastic materials
About Our Company – Learn more about our supply capabilities and quality assurance
Technical Documents for NORYL PPO534 Resin
| Document Type | Description & Source |
|---|---|
| Manufacturer Official TDS | Complete physical, thermal, and mechanical properties of NORYL PPO534 |
| Manufacturer Official SDS | GHS-compliant safety documentation |
| COA (Certificate of Analysis) | Batch-specific quality certification |
| UL Yellow Card | E45587 – UL safety certification |
| Chemical Resistance Properties | NORYL Resin chemical resistance documentation |
Request any document above by:
Email: ruiqingchem@gmail.com
Online form: Our contact page
We reply within one working business day. Please clearly state product (NORYL PPO534) and document type you require.
FAQ about NORYL PPO534 Resin
Q1: What is NORYL PPO534?
A: NORYL PPO534 is a non-reinforced blend of polyphenylene ether (PPE) and polystyrene (PS) from SABIC. It is a high heat injection moldable grade that exhibits high impact strength, dimensional stability, hydrolytic stability, and very low moisture absorption.
Q2: What are the key features of NORYL PPO534?
A: It offers non-reinforced PPE/PS blend, high heat resistance (HDT 160°C), high impact strength (137 J/m notched Izod), dimensional stability, hydrolytic stability, very low moisture absorption (0.03%), UL94 V-1 flame rating, RoHS compliance, and No PFAS intentionally added.
Q3: What are the typical applications for NORYL PPO534?
A: Typical applications include compounding and masterbatch production, material handling equipment, drone components, electrical and electronic components, consumer electronics (mobile phones, computers, tablets), and various injection molded components.
Q4: What is the flame rating of NORYL PPO534?
A: UL94 V-1 at 1.5mm thickness.
Q5: What is the heat deflection temperature of NORYL PPO534?
A: The heat deflection temperature at 1.82 MPa (264 psi, 6.4mm, unannealed) is 160°C.
Q6: What is the recommended processing method for NORYL PPO534?
A: NORYL PPO534 is designed for injection molding.
Q7: What is the recommended drying condition for NORYL PPO534?
A: Dry at 100 – 120°C for 3 – 4 hours prior to processing.
Q8: What is the recommended melt temperature for NORYL PPO534?
A: 290 – 320°C.
Q9: What is the specific gravity of NORYL PPO534?
A: The specific gravity is 1.08 g/cm³ (1,080 kg/m³).
Q10: What is the UL Yellow Card number for NORYL PPO534?
A: E45587 – SABIC JAPAN L L C.
Q11: What regions is NORYL PPO534 available in?
A: It is available in the Asia Pacific region.
Q12: What is the lead time for orders?
A: Regular orders ship within 7-10 working days after payment confirmation. Large-volume orders can be negotiated separately.
CTA (Call to Action)
Ready to order NORYL PPO534?
To get a precise quotation and professional technical support, please share:
-
Required quantity (kg)
-
Destination port or delivery address
-
Target application (compounding, material handling, electronics, etc.)
-
Document requirement (TDS, SDS, COA, UL docs, etc.)
Sample Policy:
-
Samples are for laboratory validation tests only, not for production use.
-
Buyer bears international sample-shipping freight.
-
If bulk-product performance deviates from sample reference, manufacturer official TDS serves as the authoritative benchmark.
Take action now:
-
📧 Email Us – ruiqingchem@gmail.com
-
📝 Send Inquiry – Use our quick inquiry form
-
💬 Live Chat – Click the bottom-right chat widget to speak directly with our team
After-Sales Support
| Service | Details |
|---|---|
| Quality Inspection Period | All quality-related claims must be submitted within 7 working days after delivery, supported by test data and photographic evidence. |
| Return / Exchange Policy | Confirmed product defects caused by our side trigger replacement or refund. Terms and conditions apply. |
| Logistics Damage | Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim-document preparation. |
| Technical Support | Remote technical guidance available. On-site troubleshooting can be arranged upon special request. |
| Export Documentation | We supply commercial invoice, packing list, bill of lading, COA, and additional compliance certificates on request. |
Disclaimer
DISCLAIMER: All technical data is referenced from original manufacturer typical values for NORYL PPO534. Our company acts as authorized distributor/trader rather than original manufacturer. Final performance depends on processing conditions and part design. Buyers shall independently validate product suitability for individual applications. Our firm bears no liability for product failure caused by improper processing or improper usage. Always reference the latest manufacturer official TDS of NORYL PPO534 as the definitive specification.