描述
Fortron FX40T1 is an unfilled, impact-modified high toughness polyphenylene sulfide (PPS) grade from Celanese Corporation . This grade is specifically designed to provide significantly improved toughness and impact resistance compared to standard PPS grades, making it ideal for applications where durability and reliability are critical.
As a linear, semi-crystalline PPS, Fortron FX40T1 provides high dimensional stability, excellent chemical resistance, and very low moisture absorption . The impact modification allows the material to withstand higher stress and strain without brittle failure, while maintaining the inherent flame retardancy and thermal stability of PPS.
The material exhibits a Charpy notched impact strength of 50 kJ/m² at 23°C , which is significantly higher than standard unfilled PPS grades. This exceptional toughness is combined with a tensile modulus of 2.42 GPa and a tensile strength at break of 48 MPa .
For more PPS grades and technical information, please visit our PPS/Polyphenylene Sulfide product page. You can also explore Celanese’s official Fortron PPS portfolio for additional manufacturer insights.
Key Features of Fortron FX40T1
-
Unfilled Grade – Pure PPS with impact modification for enhanced toughness
-
Impact Modified – Significantly improved toughness and impact resistance; Charpy notched impact of 50 kJ/m² at 23°C and 10 kJ/m² at -30°C
-
Good Mechanical Properties – Tensile modulus of 2,420 MPa; tensile strength of 48 MPa; flexural modulus of 2,800 MPa; flexural strength of 85 MPa at 3.5% strain
-
High Elongation – Excellent ductility due to impact modification
-
Excellent Heat Resistance – Melting point ~280°C; continuous use temperature up to 240°C
-
Inherent Flame Retardancy – V-0 flame retardant (halogen-free)
-
Excellent Chemical Resistance – Insoluble in all known solvents below 200°C; resists acids, bases, and fuels
-
Very Low Moisture Absorption – <0.02% water absorption, ensuring dimensional stability
-
Versatile Processing – Suitable for injection molding, extrusion, and blow molding
-
Global Supply – Available across North America, Europe, Asia Pacific, Latin America, Africa & Middle East
-
Good Electrical Properties – Volume resistivity >10¹³ Ω·m; dielectric constant ~4.1 at 1MHz
Typical Applications for Fortron FX40T1
| Industry | Typical Components & Considerations |
|---|---|
| Automotive | Under-hood components, clips, fasteners, connectors, sensors – requiring toughness and chemical resistance |
| Industrial | Pump and valve components, chemical processing equipment, high-pressure parts |
| Electrical & Electronics | Connectors, coil bobbins, relay housings – requiring V-0 flammability and toughness |
| Consumer Goods | Durable components requiring impact resistance and heat stability |
| Blow Molding | Hollow components – utilizing good melt strength and toughness |
Typical Properties of Fortron FX40T1
| Property | Value | Test Method |
|---|---|---|
| Physical | ||
| Density | ~1.3 g/cm³ | ISO 1183 |
| Mechanical | ||
| Tensile Modulus | 2,420 MPa | ISO 527-1/-2 |
| Tensile Strength at Break | 48 MPa | ISO 527-1/-2 |
| Flexural Modulus | 2,800 MPa | ISO 178 |
| Flexural Strength (3.5% strain) | 85 MPa | ISO 178 |
| Impact | ||
| Charpy Notched Impact (23°C) | 50 kJ/m² | ISO 179/1eA |
| Charpy Notched Impact (-30°C) | 10 kJ/m² | ISO 179/1eA |
| Poisson’s Ratio | 0.411 | ISO 527 |
| Processing | ||
| Drying Temperature | 130°C | |
| Drying Time | 2 – 4 hours | |
| Suggested Max Moisture | ≤ 0.02% | |
| Melt Temperature (Optimum) | 330°C | |
| Melt Temperature Range | 310 – 340°C | |
| Mold Temperature (Optimum) | 120°C | |
| Mold Temperature Range | 80 – 160°C | |
| Screw Tangential Speed | 0.2 – 0.3 m/s | |
| Hold Pressure Range | 30 – 70 MPa | |
| Back Pressure | ≤ 3.5 MPa |
Important Notes on Typical Data
📌 Values are typical – The data listed above is sourced from manufacturer data sheets for reference only and does not constitute binding product specifications for Fortron FX40T1.
📌 Batch variations – Batch-to-batch deviations may exist. For critical applications, validate performance with batch-specific COA certificates.
📌 Final performance – Actual performance depends on processing conditions and part design. Refer to ISO testing standards for detailed methodology.
📌 Authoritative reference – The manufacturer’s official TDS shall serve as the definitive technical reference for Fortron FX40T1. Request the latest official TDS from our sales team.
Critical Processing Warnings for Fortron FX40T1
⚠️ Drying Requirement – Fortron FX40T1 requires drying prior to processing. Predrying in a dehumidified air dryer at 130°C for 2–4 hours is recommended . The time between drying and processing should be as short as possible.
⚠️ Moisture Control – Maximum residual moisture content should be ≤ 0.02% . Proper drying is essential to prevent void formation and ensure optimal part quality.
⚠️ Melt Temperature – The recommended melt temperature range is 310–340°C, with an optimum of 330°C . Avoid exceeding 340°C to prevent material degradation.
⚠️ Mold Temperature – A wide range of mold temperatures (80–160°C) is possible, with an optimum of 120°C . Higher mold temperatures promote higher crystallinity and better heat resistance.
⚠️ Impact Modified Grade – This grade is specifically formulated for high toughness and impact resistance . Processing parameters should be optimized to maintain impact modification performance.
⚠️ Versatile Processing – This grade is suitable for injection molding, extrusion, and blow molding . For extrusion and blow molding, adjust parameters based on specific equipment and final product requirements.
⚠️ Storage – Store in original, sealed packaging in a cool, dry place away from direct sunlight. For subsequent storage, the material should be stored dry until processed.
Comparison: Fortron FX40T1 vs. Fortron FX32T4
| Feature | Fortron FX40T1 | Fortron FX32T4 |
|---|---|---|
| Filler | Unfilled | Unfilled |
| Key Feature | High toughness impact modified | Impact modified + High flow |
| Tensile Modulus | 2,420 MPa | 2,100 MPa |
| Tensile Strength | 48 MPa | 46 MPa |
| Flexural Modulus | 2,800 MPa | ~2,200 MPa |
| Charpy Notched Impact (23°C) | 50 kJ/m² | 10 kJ/m² |
| Charpy Notched Impact (-30°C) | 10 kJ/m² | — |
| Mold Temperature Range | 80 – 160°C | 70 – 160°C |
| Processing | Injection, Extrusion, Blow Molding | Injection Molding |
Related Products
-
PPS/Polyphenylene Sulfide – View our full range of PPS products
-
Fortron FX32T4 – Impact modified unfilled PPS with high flow
-
Fortron FX20T1 – Impact modified unfilled PPS with good flowability
-
Fortron 0205 – Medium viscosity unfilled PPS for compounding
-
Explore Engineering Plastics – Browse all engineering plastic materials
-
About Our Company – Learn more about our supply capabilities and quality assurance
Technical Documents for Fortron FX40T1
| Document Type | Description & Source |
|---|---|
| Manufacturer Official TDS | Complete physical, thermal, and mechanical properties of Fortron FX40T1 |
| Manufacturer Official SDS | GHS-compliant safety documentation |
| COA (Certificate of Analysis) | Batch-specific quality certification for Fortron FX40T1 |
| UL Yellow Card | UL safety certification |
Request any document above by:
📧 Email: ruiqingchem@gmail.com
📝 Online form: Our contact page
We reply within one working business day. Please clearly state product (Fortron FX40T1) and document type you require.
FAQ about Fortron FX40T1
Q1: What is Fortron FX40T1?
A: Fortron FX40T1 is an unfilled, impact-modified high toughness polyphenylene sulfide (PPS) grade from Celanese Corporation, designed for applications requiring superior impact resistance and durability .
Q2: What are the key features of Fortron FX40T1?
A: Unfilled; impact-modified high toughness; Charpy notched impact 50 kJ/m² at 23°C; tensile modulus 2,420 MPa; flexural modulus 2,800 MPa; excellent chemical resistance; inherent flame retardancy; versatile processing .
Q3: What are the typical applications for Fortron FX40T1?
A: Automotive under-hood components, electrical and electronic components, industrial pump and valve parts, and blow molded components .
Q4: What is the recommended drying condition for Fortron FX40T1?
A: Dry at 130°C for 2–4 hours using a dehumidified air dryer. Maximum residual moisture should be ≤ 0.02% .
Q5: What is the tensile modulus of Fortron FX40T1?
A: 2,420 MPa (2.42 GPa) .
Q6: What is the HDT of Fortron FX40T1?
A: The continuous use temperature is up to 240°C. HDT data for this specific grade should be confirmed from the official TDS .
Q7: What regions is Fortron FX40T1 available in?
A: North America, Europe, Asia Pacific, Latin America, Africa & Middle East .
Q8: Is Fortron FX40T1 flame retardant?
A: Yes, it is inherently flame-retardant (V-0) .
Q9: Is Fortron FX40T1 suitable for blow molding?
A: Yes, this grade is suitable for blow molding in addition to injection molding and extrusion .
Q10: What is the Charpy notched impact strength of Fortron FX40T1?
A: 50 kJ/m² at 23°C and 10 kJ/m² at -30°C .
Q11: Is Fortron FX40T1 RoHS compliant?
A: Yes, it complies with RoHS and other environmental regulations .
Q12: What is the Poisson’s ratio of Fortron FX40T1?
A: 0.411 .
CTA (Call to Action)
Ready to order Fortron FX40T1?
To get a precise quotation and professional technical support for Fortron FX40T1, please share:
-
Required quantity (kg)
-
Destination port or delivery address
-
Target application (injection molding, extrusion, blow molding, automotive, electronics, etc.)
-
Document requirements (TDS, SDS, COA, UL docs)
Sample Policy:
-
Samples of Fortron FX40T1 are for laboratory validation tests only, not for production use.
-
Buyer bears international sample-shipping freight.
-
If bulk-product performance deviates from sample reference, the manufacturer’s official TDS serves as the authoritative benchmark.
Take action now:
📧 Email Us – ruiqingchem@gmail.com
📝 Send Inquiry – Use our quick inquiry form
💬 Live Chat – Click the bottom-right chat widget to speak directly with our team
After-Sales Support
| Service | Details |
|---|---|
| Quality Inspection Period | All quality-related claims must be submitted within 7 working days after delivery, supported by test data and photographic evidence. |
| Return / Exchange Policy | Confirmed product defects caused by our side trigger replacement or refund. Terms and conditions apply. |
| Logistics Damage | Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim-document preparation. |
| Technical Support | Remote technical guidance available. On-site troubleshooting can be arranged upon special request. |
| Export Documentation | We supply commercial invoice, packing list, bill of lading, COA, and additional compliance certificates on request. |
Disclaimer
DISCLAIMER: All technical data is referenced from original manufacturer typical values for Fortron FX40T1 . Our company acts as supplier/trader rather than original manufacturer. Final performance depends on processing conditions and part design. Buyers shall independently validate product suitability for individual applications. Our firm bears no liability for product failure caused by improper processing or improper usage. Always reference the latest manufacturer official TDS of Fortron FX40T1 as the definitive specification.