Hostaform TF-10XAP – Low Emission Impact Modified POM-C

基础信息

品名
Hostaform TF-10XAP
牌号
TF-10XAP
厂商
Celanese
材料类型
Polyoxymethylene (POM) Copolymer
产品形态
Resin Pellets
特点
Low emission, improved flow, impact modified grade providing optimum performance in general purpose injection molding, primarily for the interior automotive market

描述

Hostaform TF-10XAP is a low emission, improved flow, impact modified POM‑C (Polyoxymethylene Copolymer) grade, genuinely manufactured by Celanese and imported as original product. As an authorized distributor and trader, we supply genuine material with full traceability and direct access to official Celanese technical documentation.

This unfilled acetal copolymer is an impact modified grade providing optimum performance in general purpose injection molding, primarily for the interior automotive market. The improved flow characteristics (MVR 13 cm³/10min) enable efficient filling of complex part geometries while maintaining excellent mechanical properties.

Hostaform TF-10XAP delivers overall excellent performance with improved impact in many applications. The “XAP” designation indicates Celanese’s low emission technology, making it especially suitable for automotive interior applications with strict cabin air quality requirements. It complies with RoHS regulations.

Hostaform TF-10XAP is a very hard and rigid, heavy-metal free POM copolymer grade that exhibits outstanding chemical resistance (solvents, fuels & strong alkalis), hydrolysis resistance, fatigue resistance, creep resistance, moisture resistance, and stress cracking resistance. It also exhibits toughness, good heat distortion temperature (75°C at 1.8 MPa), very good slip/wear properties, excellent resilience, and low moisture absorption. Available in natural and black (14 BLACK), this grade is supplied globally across North America, Europe, Asia Pacific, South and Central America, and Near East/Africa. With regular stock availability, we support both trial orders and large‑volume bulk shipments for automotive and general purpose end‑users.

Key Features of Hostaform TF-10XAP

  • Impact Modified – Impact modified grade providing improved impact resistance for demanding applications

  • Low Emission Technology – XAP low emission technology, especially suitable for automotive interior applications with strict cabin air quality requirements

  • Improved Flow / Easy Processing – MVR of 13 cm³/10min (190°C/2.16kg), providing excellent flow for injection molding of complex parts

  • High Ductility – Yield strain of 13% and nominal strain at break of >50%

  • Good Stiffness – Tensile modulus of 1750 MPa

  • Good Impact Resistance – Charpy notched impact strength of 8 kJ/m² at 23°C and 5 kJ/m² at -30°C

  • Good Heat Resistance – Melting temperature of 165°C and heat deflection temperature of 75°C at 1.8 MPa

  • Automotive Interior Focus – Primarily designed for the interior automotive market

  • RoHS Compliant – Meets RoHS environmental compliance requirements

  • Heavy‑Metal Free – Environmentally friendly formulation

  • Contains Release Agent – Facilitates easy demolding during processing

  • Global Availability – Available in North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Typical Applications for Hostaform TF-10XAP

Industry Typical Components & Considerations
Automotive Interior Interior components, instrument panel parts, air vent louvers, interior trim clips, door handles, seat belt components. Low emission technology ensures compliance with cabin air quality standards.
Automotive Gears, bearings, fuel system components, door locks, seat belt systems
Electrical & Electronics Connectors, switches, coil formers, precision housings, low VOC components
Industrial Machinery Gears, cams, guide rails, pump valves, conveyor rollers, fasteners
Consumer Goods Sporting equipment, furniture mechanisms, personal care devices, toys
Precision Engineering Precision gears, bearings, connectors, fasteners, snap-fit components

Explore our full range of engineering plastics solutions for more industry‑specific case studies. See also our full POM product portfolio .

Material Advantages of Hostaform TF-10XAP

What makes Hostaform TF-10XAP the preferred material for automotive interior and general purpose injection molding applications? Below are its core practical advantages:

Impact Modified for Improved Toughness
Hostaform TF-10XAP is an impact modified grade providing improved impact resistance for demanding applications. With Charpy notched impact strength of 8 kJ/m² at 23°C and 5 kJ/m² at -30°C, it delivers reliable performance in applications where standard POM grades would fall short.

Low Emission Technology for Automotive Interiors
The “XAP” designation indicates Celanese’s low emission technology, making it especially suitable for automotive interior applications with strict cabin air quality requirements. This enables compliance with the most stringent automotive interior air quality standards.

Improved Flow for Complex Part Geometries
With an MVR of 13 cm³/10min and improved flow characteristics, this grade enables efficient filling of complex part geometries, reducing injection pressure and cycle time while minimizing internal stress in parts. The improved flow over standard grades makes it ideal for thin-wall and intricate designs.

High Ductility with Good Stiffness
With a tensile modulus of 1750 MPa, yield stress of 48 MPa, yield strain of 13%, and nominal strain at break of >50%, Hostaform TF-10XAP offers a balance of stiffness and ductility—maintaining structural integrity while providing the flexibility needed for impact resistance.

Good Heat Resistance
Melting temperature of 165°C and heat deflection temperature of 75°C at 1.8 MPa ensure thermal stability during processing and service.

Excellent Chemical & Environmental Resistance
Outstanding resistance to solvents, fuels, strong alkalis, hydrolysis, fatigue, creep, moisture, and stress cracking.

RoHS Compliant
Hostaform TF-10XAP complies with RoHS environmental regulations.

Heavy‑Metal Free
Environmentally friendly, heavy‑metal‑free formulation.

Batch‑to‑Batch Consistency
Celanese manufactures this grade under strict ISO quality standards for consistent property across shipments.

Reliable Supply
We maintain active inventory and stable supply chains for Hostaform TF-10XAP. For more supply‑chain details, visit our company background page .

Typical Properties (ISO Standards)

Typical properties of Hostaform TF-10XAP measured to ISO standards are listed below:

Property Test Standard Typical Value Unit
Physical Properties
Density ISO 1183 1380 kg/m³
Melt Volume Flow Rate (MVR) ISO 1133 (190°C/2.16kg) 13 cm³/10min
Molding Shrinkage, Parallel ISO 294-4, 2577 2.1 %
Molding Shrinkage, Normal ISO 294-4, 2577 1.9 %
Mechanical Properties
Tensile Modulus ISO 527-1/-2 1750 MPa
Tensile Stress at Yield (50mm/min) ISO 527-1/-2 48 MPa
Tensile Strain at Yield (50mm/min) ISO 527-1/-2 13 %
Flexural Modulus ISO 178 1700 MPa
Flexural Stress at 3.5% ISO 178 46 MPa
Charpy Notched Impact (23°C) ISO 179/1eA 8 kJ/m²
Charpy Notched Impact (-30°C) ISO 179/1eA 5 kJ/m²
Hardness, Rockwell M-scale ISO 2039-2 65
Poisson’s Ratio 0.41
Thermal Properties
Melting Temperature (10°C/min) ISO 11357-1/-3 165 °C
Heat Deflection Temp (1.8 MPa) ISO 75-1/-2 75 °C
Heat Deflection Temp (0.45 MPa) ISO 75-1/-2 139 °C
Processing
Drying Recommended Recommended
Drying Temperature 100 °C
Drying Time 3 – 4 h
Optimum Melt Temperature 190 °C
Melt Temperature Range 180 – 200 °C
Optimum Mold Temperature 90 °C
Mold Temperature Range 80 – 100 °C
Ejection Temperature 133 °C
Hold Pressure Range 60 – 120 MPa

Important Notes on Typical Data:

  1. Values listed are typical and sourced from Celanese official data sheets for Hostaform TF-10XAP. They do not constitute binding product specification.

  2. Batch‑to‑batch deviations may exist. For critical applications, validate performance with batch‑specific COA certificate.

  3. Final part performance depends on component design, processing parameters and end‑use environment.

  4. Celanese original TDS shall serve as definitive technical reference. Request the latest official Hostaform TF-10XAP TDS from our sales team.

Processing Guidelines (Injection Molding)

Recommended processing parameters for Hostaform TF-10XAP:

Parameter Recommended Setting
Drying Recommended Recommended
Drying Temperature 100°C
Drying Time (Dehumidified Dryer) 3 – 4 hours
Max. Processing Moisture Content ≤0.2%
Zone 1 (Rear) Temperature 170 – 180°C
Optimum Melt Temperature 190°C
Min. Melt Temperature 180°C
Max. Melt Temperature 200°C
Screw Tangential Speed ≤0.3 m/s
Optimum Mold Temperature 90°C
Min. Mold Temperature 80°C
Max. Mold Temperature 100°C
Hold Pressure Range 60 – 120 MPa
Back Pressure 2 MPa
Ejection Temperature 133°C

Critical Processing Warnings for Hostaform TF-10XAP:

  • Improved Flow Processing: With MVR of 13 cm³/10min and improved flow characteristics, Hostaform TF-10XAP is designed for efficient filling of complex part geometries. Adjust cycle parameters to maximize throughput while maintaining part quality.

  • Drying: Drying is recommended at 100°C for 3-4 hours. If material has come into contact with moisture through improper storage, drying is necessary to prevent splay and odor.

  • Low Emission Property: To maintain XAP low emission characteristics, avoid contamination and ensure proper processing conditions.

  • Thermal Degradation Risk: POM‑based material can decompose under excessive heat and release formaldehyde vapors. Guarantee sufficient ventilation; avoid overly long barrel residence times. Max. melt temperature 200°C.

  • Material Purity Requirement: Strictly prevent cross‑contamination with other polymer grades. Contamination will degrade the impact-modified and low emission properties.

  • Regrind / Recycled Material Notice: We do not recommend adding regrind for this specialty grade. Reprocessing may compromise the impact properties and XAP low emission characteristics. If regrind usage is mandatory, keep percentage below 10% and complete pre‑validation testing first.

  • Storage Guidance: Store pellets in cool, dry conditions; keep sealed in original factory packaging whenever possible to maintain low emission characteristics.

Related Products

Technical Documents

We provide complete supporting documentation for material selection and compliance verification.

Document Type Description & Source
Celanese Official TDS Complete physical, thermal, mechanical and processing properties of Hostaform TF-10XAP, issued by Celanese original.
Celanese Official SDS GHS‑compliant chemical safety documentation, original Celanese document.
Celanese Distributor Authorization Certificate Proof of our authorized‑distributor qualification for Celanese Hostaform series, available upon request.
RoHS Compliance Declaration RoHS compliance documentation.
UL Yellow Card UL flammability rating documentation.
Processing & Molding Guide Detailed molding operation guidance for impact modified low emission POM.

Request any document above by:

  • Email: ruiqingchem@gmail.com

  • Online form: Our contact page

We reply within one working business day. Please clearly state material grade (Hostaform TF-10XAP) and document type you require.

External Reference

For further authoritative information, please refer to the official Celanese Hostaform product portal and the latest material datasheets for Hostaform TF-10XAP.

Key technical standards referenced in this document include:

  • ISO 1043 / ISO 11469 – Resin identification and part marking

  • ISO 1183 – Density measurement

  • ISO 527-1/-2 – Tensile properties

  • ISO 178 – Flexural properties

  • ISO 179/1eA – Charpy notched impact resistance

  • ISO 75-1/-2 – Heat deflection temperature

  • ISO 1133 – Melt volume-flow rate

  • ISO 11357-1/-3 – Melting temperature

  • ISO 294-4, 2577 – Mold shrinkage

  • ISO 2039-2 – Rockwell hardness

Our technical team can supply relevant standard excerpts for your engineering reference.

FAQ

Q1: What is Hostaform TF-10XAP and what is it used for?
A: Hostaform TF-10XAP is a low emission, improved flow, impact modified POM‑C (Polyoxymethylene Copolymer) injection molding grade. It provides optimum performance in general purpose injection molding, primarily for the interior automotive market. It is widely used in automotive interior components (instrument panels, air vents, interior trim clips, door handles), automotive (gears, bearings, fuel system components, door locks, seat belt systems), electrical & electronics (connectors, switches, housings), industrial machinery, and consumer goods.

Q2: What does “TF-10XAP” mean in the grade name?
A: TF indicates a specific formulation within the Hostaform series (impact modified grade). 10 denotes the product series. XAP denotes Celanese’s low emission technology for reduced VOC emissions and low odor, making it especially suitable for automotive interior applications.

Q3: What makes this grade different from standard POM grades?
A: Hostaform TF-10XAP is an impact modified grade with improved flow characteristics and low emission technology. It provides improved impact resistance over standard POM grades while maintaining good stiffness (1750 MPa tensile modulus). The improved flow enables efficient filling of complex part geometries.

Q4: What are the key mechanical properties?
A: Tensile modulus 1750 MPa, tensile stress at yield 48 MPa, tensile strain at yield 13%, Charpy notched impact strength 8 kJ/m² (23°C) / 5 kJ/m² (-30°C), flexural modulus 1700 MPa, melting temperature 165°C, and heat deflection temperature 75°C at 1.8 MPa.

Q5: What is the MVR of this material?
A: Melt‑volume‑flow‑rate equals 13 cm³/10min measured under 190°C / 2.16 kg test condition.

Q6: Is this material suitable for automotive applications?
A: Yes. Hostaform TF-10XAP is primarily designed for the interior automotive market with low emission technology. It is also suitable for general automotive components including gears, bearings, and fuel system components.

Q7: What colors are available?
A: Hostaform TF-10XAP is available in natural and 14 BLACK.

Q8: Is drying required before processing?
A: Drying is recommended at 100°C for 3-4 hours. If material has come into contact with moisture through improper storage, drying is necessary to prevent splay and odor.

Q9: What are recommended processing‑temperature windows?
A: Optimum melt temperature: 190°C; Melt temperature range: 180-200°C. Optimum mold temperature: 90°C; Mold temperature range: 80-100°C. Zone 1 (rear) temperature: 170-180°C.

Q10: What is the density of this material?
A: The density is 1380 kg/m³.

Q11: What regions is this material available in?
A: Hostaform TF-10XAP is available in North America, Europe, Asia Pacific, South and Central America, and Near East/Africa.

Q12: Is this material RoHS compliant?
A: Yes, Hostaform TF-10XAP complies with RoHS regulations.

Q13: Can I buy this material and what is lead‑time?
A: Yes. Submit your inquiry via our quick inquiry form or email ruiqingchem@gmail.com, specify quantity, application and delivery address. Regular orders 1‑5 tons ship within 7‑10 working days after payment confirmation. Large‑volume or urgent orders can be negotiated separately.

Q14: What are limitations?
A: POM‑C does not resist strong mineral acids, powerful oxidizing agents, or continuous exposure to hot water >80°C. Consult our technical team for chemical‑compatibility data for your exact working environment.

CTA (Call to Action)

Ready to order Hostaform TF-10XAP?

To get precise quotation and professional technical support, please share these details:

  • Required quantity (kg or tons)

  • Destination port or delivery address

  • Target application and part brief (automotive interior, general purpose injection molding, etc.)

  • Color requirements (natural, 14 BLACK, or custom color)

  • Core performance requirements (impact resistance, low emission, flowability, etc.)

  • Document requirement (TDS, SDS, RoHS compliance, UL Yellow Card, etc.)

Sample Policy:

  • Samples are for laboratory validation tests only, not for production use.

  • Buyer bears international sample‑shipping freight.

  • If bulk‑material performance deviates from sample reference, Celanese official TDS serves as authoritative benchmark.

Take action now:

  • Send Inquiry – Use our quick inquiry form

  • Email Us – ruiqingchem@gmail.com

  • Live Chat – Click bottom‑right chat widget to speak directly with our team

After-Sales Support

Service Details
Quality Inspection Period All quality‑related claims must be submitted within 7 working‑days after delivery, supported by test data and photographic evidence.
Return / Exchange Policy Confirmed material defects caused by our side trigger replacement or refund. Terms and conditions apply. Please check our full Terms & Conditions.
Logistics Damage Report shipping damage directly to carrier immediately upon goods receipt. We assist with claim‑document preparation.
Technical Support Remote technical guidance available. On‑site molding troubleshooting service can be arranged upon special request.
Export Documentation We supply standard export documents: commercial invoice, packing list, bill of lading, COA. Additional compliance certificates (e.g., RoHS compliance, UL Yellow Card) can be provided on request.

Disclaimer

DISCLAIMER: All technical data is referenced from original Celanese typical values for Hostaform TF-10XAP. Our company acts as authorized distributor/trader rather than original manufacturer. Final component performance depends on part geometry, processing setup and end‑use environment. Buyers shall independently validate material suitability for individual applications. Our firm bears no liability for finished‑part failure caused by improper design or improper processing. Always reference latest Celanese official TDS of Hostaform TF-10XAP as definitive specification.

Technical Documents

Download technical data sheets, safety data sheets and certificates for this material.

TDS Files

Technical document available for review or download.

0 Files
No TDS file uploaded yet.

MSDS Files

Technical document available for review or download.

0 Files
No MSDS file uploaded yet.