描述
VESTAMID LX9012 T8 is a heat-stabilized and light-resistant polyamide 12 compound from Evonik Operations GmbH developed especially for the extrusion and co-extrusion of ski upper films and decorative films.
The grade combines the engineering performance of semi-crystalline PA12 with the optical and surface properties required for visible sports and lifestyle components. Films produced from VESTAMID LX9012 T8 are described by Evonik as having high transparency, good screen-printing and sublimation-printing capability, outstanding scratch resistance and excellent impact strength at low temperatures.
These properties are especially important for ski upper films. A ski surface must remain visually attractive while being exposed to snow, moisture, abrasion, impact and low temperatures. VESTAMID LX9012 T8 provides a durable PA12 surface that can protect printed designs while maintaining a clean transparent or translucent appearance.
Decoration on the bottom side of injection-molded sports shoe soles is another published application. This allows the material to support visible graphics and decorative effects in products where toughness and scratch resistance are also required.
The semi-crystalline PA12 matrix absorbs only small quantities of water. Published water absorption is approximately 1.5%, while humidity absorption is approximately 0.8%. Low moisture uptake helps products maintain dimensional stability and impact performance as ambient humidity changes.
PA12 also offers a naturally low coefficient of friction and good general chemical resistance. These characteristics help improve the surface durability and handling performance of decorative films and molded sports components.
Current grade data lists both film extrusion and injection molding as processing methods. The grade is supplied as cylindrical granules in moisture-proof packaging and is ready for processing when the packaging remains intact.
For more PA12 materials, visit our PA12 Polyamide 12 Product Category →.
For manufacturer information about VESTAMID materials, visit the Official Evonik VESTAMID Page →.
Key Features of VESTAMID LX9012 T8
| Feature | Benefit |
|---|---|
| Transparent / Translucent Appearance | Supports visible decorative surfaces and printed graphics |
| Heat Stabilized | Helps maintain properties during processing and service |
| Light / UV / Weathering Stabilized | Supports outdoor sports and lifestyle applications |
| Film Extrusion Grade | Developed specifically for extrusion and co-extrusion of decorative films |
| Screen Printable | Supports logos, graphics and decorative printing |
| Sublimation Printable | Allows transferred graphics and color effects |
| Outstanding Scratch Resistance | Helps visible surfaces retain appearance during use |
| Excellent Low-Temperature Impact | Supports ski and outdoor applications exposed to cold environments |
| Low Water Absorption | Reduces humidity-related dimensional change |
| Low Coefficient of Friction | Provides a smooth, low-friction surface |
| Good Chemical Resistance | Supports exposure to common environmental and household media |
| Fatigue / Wear Resistance | Useful for repeatedly handled sports and lifestyle components |
The combination of transparency, printability and engineering toughness is the main reason to choose VESTAMID LX9012 T8 instead of a conventional decorative film polymer.
Typical Applications for VESTAMID LX9012 T8
VESTAMID LX9012 T8 is primarily designed for visible sports and decorative film applications.
| Application Area | Typical Use |
|---|---|
| Ski Upper Films | Transparent protective upper layers with printed graphics |
| Decorative Films | Extruded and co-extruded PA12 films requiring scratch resistance |
| Printed Sports Films | Screen-printed or sublimation-printed decorative surfaces |
| Sports Shoe Sole Decoration | Decoration on the bottom side of injection-molded soles |
| Sports Equipment Components | Visible parts requiring low-temperature impact strength |
| Lifestyle Products | Transparent or translucent parts with durable surface appearance |
| Protective Decorative Layers | Films combining visual design with abrasion resistance |
| Injection-Molded Decorative Parts | Selected molded components requiring PA12 toughness |
Evonik specifically identifies ski upper films, decorative films and sports shoe sole decoration as applications for VESTAMID LX9012 T8, so these uses should remain the main commercial positioning of the grade.
Typical Properties of VESTAMID LX9012 T8
Physical & Rheological Properties
| Property | Typical Value | Test Method |
|---|---|---|
| Density | 1.01 g/cm³ | ISO 1183 |
| Water Absorption | 1.5% | Similar to ISO 62 |
| Humidity Absorption | 0.8% | Similar to ISO 62 |
| Shore D Hardness | 71 | ISO 7619-1 |
| Melt Volume-Flow Rate (MVR) | 22 cm³/10 min | ISO 1133 |
| MVR Test Condition | 220°C / 10 kg | — |
| Molding Shrinkage – Parallel | 1.3% | ISO 294-4 / 2577 |
| Molding Shrinkage – Normal | 1.3% | ISO 294-4 / 2577 |
| Structure | Semi-crystalline | Manufacturer information |
| Appearance | Natural Color / Transparent to Translucent | Manufacturer information |
The balanced 1.3% / 1.3% shrinkage supports relatively uniform dimensional behavior in molded test specimens.
Mechanical Properties
| Property | Typical Value | Test Method |
|---|---|---|
| Tensile Modulus | 1,100 MPa | ISO 527 |
| Yield Stress | 35 MPa | ISO 527 |
| Yield Strain | 5% | ISO 527 |
| Nominal Strain at Break | >50% | ISO 527 |
| Charpy Impact Strength, 23°C | No Break | ISO 179/1eU |
| Charpy Impact Strength, -30°C | No Break | ISO 179/1eU |
| Charpy Notched Impact, 23°C | 13 kJ/m² | ISO 179/1eA |
| Charpy Notched Impact, -30°C | 15 kJ/m² | ISO 179/1eA |
The low-temperature performance is particularly important. VESTAMID LX9012 T8 retains a no-break result in unnotched Charpy testing at -30°C, supporting ski and outdoor sports applications.
Thermal & Flammability Properties
| Property | Typical Value | Test Method |
|---|---|---|
| Melting Temperature | 176°C | ISO 11357-1/-3 |
| Glass Transition Temperature | 39°C | ISO 11357-1/-2 |
| HDT @ 1.80 MPa | 45°C | ISO 75-1/-2 |
| HDT @ 0.45 MPa | 120°C | ISO 75-1/-2 |
| Vicat Softening Temperature B | 130°C | ISO 306 |
| CTE – Parallel | 130 × 10⁻⁶/K | ISO 11359-1/-2 |
| Flammability @ 1.5 mm nominal | HB | IEC 60695-11-10 |
| Tested Thickness | 1.6 mm | — |
The grade is not positioned as a flame-retardant material. Its principal value lies in transparency, surface durability, printability and low-temperature toughness.
Electrical Properties
| Property | Typical Value | Test Method |
|---|---|---|
| Relative Permittivity, 100 Hz | 3.8 | IEC 62631-2-1 |
| Relative Permittivity, 1 MHz | 3.0 | IEC 62631-2-1 |
| Dissipation Factor, 100 Hz | 530 × 10⁻⁴ | IEC 62631-2-1 |
| Dissipation Factor, 1 MHz | 280 × 10⁻⁴ | IEC 62631-2-1 |
| Volume Resistivity | 1 × 10¹² Ω·m | IEC 62631-3-1 |
| Dielectric Strength | 36 kV/mm | Similar to IEC 60243-1 |
These values confirm that VESTAMID LX9012 T8 is electrically insulating, although electrical insulation is not its primary commercial application.
Why Choose VESTAMID LX9012 T8?
The main reason to choose VESTAMID LX9012 T8 is the combination of visual quality and mechanical durability.
Many transparent polymers can provide attractive appearance, but decorative sports surfaces also need impact resistance, scratch resistance and reliable performance at low temperatures. Ski products are especially demanding because they combine cold weather, moisture, repeated impact and visible graphics.
The PA12 base gives VESTAMID LX9012 T8 strong toughness while keeping water absorption low. This helps the film remain dimensionally stable and reduces the property changes associated with humidity.
Printing performance is another major advantage. Screen printing and sublimation printing allow manufacturers to place graphics, logos and complex decorative designs under or within the protective film structure.
Scratch resistance helps preserve these graphics during transportation, assembly and end use. The transparent surface can act as both a decorative and protective layer.
Low-temperature impact performance is particularly relevant to skiing. The published notched Charpy value rises from approximately 13 kJ/m² at 23°C to 15 kJ/m² at -30°C, while unnotched specimens remain no-break.
For manufacturers of skis, sports equipment and lifestyle products, VESTAMID LX9012 T8 therefore provides a focused material solution rather than a generic PA12 resin.
Processing Guidelines for VESTAMID LX9012 T8
VESTAMID LX9012 T8 is designed primarily for film extrusion and co-extrusion, while injection molding is also listed in current material data.
The grade-specific public data provides the following reference conditions:
| Processing Parameter | Published Value |
|---|---|
| Primary Process | Film Extrusion / Co-Extrusion |
| Additional Process | Injection Molding |
| MVR Test Condition | 220°C / 10 kg |
| Published Test Melt Temperature | 240°C |
| Published Test Mold Temperature | 80°C |
| Supply Form | Cylindrical pellets / granules |
| Packaging | Moisture-proof packaging |
| Shelf Life | At least 2 years at ≤30°C in original undamaged packaging |
The published 240°C melt temperature and 80°C mold temperature are material-test conditions. They should not be treated as a fixed film-extrusion recipe.
For film extrusion and co-extrusion, barrel temperatures, adapter temperature, die temperature, output rate, draw ratio, chill-roll temperature and final film thickness should be optimized for the specific production line.
Because optical appearance is a major requirement, clean material handling is especially important. Contamination, excessive residence time or thermally degraded polymer can reduce transparency and surface quality.
VESTAMID materials are supplied in moisture-proof packaging. Material from intact packaging is ready for processing. If the pellets have absorbed moisture after prolonged exposure to ambient air, drying should follow Evonik’s general VESTAMID processing recommendations.
Inside original and undamaged packaging, VESTAMID LX9012 T8 has a published shelf life of at least two years when stored dry at temperatures not exceeding 30°C.
VESTAMID LX9012 T8 vs. VESTAMID LX9012 T10
| Feature | VESTAMID LX9012 T8 | VESTAMID LX9012 T10 |
|---|---|---|
| Base Polymer | PA12 | PA12 |
| Appearance | Transparent / Translucent | Translucent |
| Primary Process | Film extrusion / co-extrusion | Injection molding |
| Primary Application | Ski upper and decorative films | Sports shoe soles |
| MVR | 22 cm³/10 min @ 220°C / 10 kg | Different injection-molding flow positioning |
| Printability | Screen and sublimation printing | Screen and sublimation printing |
| Scratch Resistance | Outstanding | Outstanding |
| Low-Temperature Impact | Excellent | Excellent |
| Main Selection Reason | Decorative film extrusion | High-flow molded shoe components |
Choose VESTAMID LX9012 T8 when the project requires extrusion or co-extrusion of transparent decorative film, especially ski upper film.
Choose VESTAMID LX9012 T10 when the project is centered on injection-molded sports shoe soles and high-flow molding performance.
Related Products
VESTAMID LX9012 T10 – Translucent PA12 optimized for injection-molded sports shoe soles.
VESTAMID LX9012 – Transparent PA12 for decorative films, ski upper films and sports applications.
VESTAMID LX9012 Bio30 – 30% bio-based PA12 for sustainable sports and lifestyle injection-molded products.
View More PA12 Polyamide 12 Materials →
Technical Documents for VESTAMID LX9012 T8
| Document Type | Description |
|---|---|
| TDS | Technical Data Sheet with physical, mechanical, thermal and electrical properties |
| SDS | Safety Data Sheet |
| COA | Batch-specific Certificate of Analysis where available |
| Processing Information | Film extrusion, co-extrusion and material-handling guidance |
| Chemical Resistance Data | General PA12 chemical resistance information |
| Application Support | Ski upper film, decorative film and sports-product evaluation |
Need technical documents for VESTAMID LX9012 T8?
📧 Email: ruiqingchem@gmail.com
📝 Online form: Contact Us →
Please state VESTAMID LX9012 T8 and the required document type when submitting your inquiry.
FAQ About VESTAMID LX9012 T8
Q1: What is VESTAMID LX9012 T8?
VESTAMID LX9012 T8 is a heat- and light-stabilized PA12 from Evonik developed especially for extrusion and co-extrusion of ski upper and decorative films.
Q2: Is VESTAMID LX9012 T8 transparent?
Yes. Evonik describes films made from the grade as having high transparency, while current product characteristics also identify transparent and translucent optical positioning.
Q3: Can VESTAMID LX9012 T8 be printed?
Yes. It provides good screen-printing and sublimation-printing performance for decorative graphics.
Q4: What is the density of VESTAMID LX9012 T8?
The typical density is approximately 1.01 g/cm³ according to ISO 1183.
Q5: What is the MVR of VESTAMID LX9012 T8?
The typical MVR is approximately 22 cm³/10 min at 220°C / 10 kg according to ISO 1133.
Q6: What is the tensile modulus of VESTAMID LX9012 T8?
The typical tensile modulus is approximately 1,100 MPa according to ISO 527.
Q7: What is the melting temperature of VESTAMID LX9012 T8?
The typical melting temperature is approximately 176°C according to ISO 11357.
Q8: How good is the low-temperature impact performance?
Unnotched Charpy specimens show no break at -30°C, while typical notched Charpy impact strength is approximately 15 kJ/m² at -30°C.
Q9: What are the published processing test conditions?
Current grade-specific data lists a 240°C melt temperature and 80°C mold temperature for test specimens. Film-extrusion settings should be optimized for the actual line.
Q10: Can you provide VESTAMID LX9012 T8 TDS, SDS and COA?
Yes. Please request the required technical documents through our Contact Page → or email ruiqingchem@gmail.com.
Request VESTAMID LX9012 T8 Price & Technical Support
For pricing, availability, technical documents or material-selection support for VESTAMID LX9012 T8, please provide:
- Required quantity
- Destination country or port
- Ski upper film, decorative film or other application
- Required film thickness
- Transparency or translucency requirement
- Printing or decoration method
- Co-extrusion structure, if applicable
- Minimum service temperature
- Scratch-resistance requirement
- Extrusion-line information
- TDS, SDS or COA requirements
- Sample requirement, if applicable
📧 Email: ruiqingchem@gmail.com
📝 Send Inquiry →