Santoprene 121-73W175 TPV UV-Resistant Profile Extrusion Grade

基础信息

品名
Santoprene 121-73W175
牌号
121-73W175
厂商
Celanese Corporation
材料类型
Thermoplastic Vulcanizate (TPV) / Thermoplastic Elastomer (TPE)
产品形态
Pellets
特点
UV-resistant black TPV, tuned for thin-wall and complex profile extrusion, excellent flex-fatigue and ozone resistance, long extrusion runs with reduced die/screen build-up, UL recognized

描述

Santoprene 121-73W175 is a soft, black, UV-resistant thermoplastic vulcanizate (TPV) from Celanese designed especially for thin-wall and complex profile extrusion.

This grade belongs to the Santoprene 121-series UV-black TPV family. In Celanese’s current product finder, Santoprene 121-73W175 is positioned as a general-purpose extrusion and molding grade with UV stability and performance specifically tuned for profile extrusion.

The material combines rubber-like flexibility and elastic recovery with the processing advantages of a thermoplastic. It is polyolefin based and can be processed on conventional thermoplastic equipment.

The most important difference between Santoprene 121-73W175 and a standard general-purpose TPV is its profile-extrusion optimization.

Celanese states that the grade is designed for extrusion of thin-wall sections with excellent definition, including geometry down to approximately 0.33 mm radius. It is also engineered to maximize production run length while minimizing material build-up on screen packs and narrow sections of extrusion dies.

This makes Santoprene 121-73W175 highly relevant to continuous automotive sealing profiles, weatherstrips, glass-run-channel components, complex sealing lips and other extruded profiles where dimensional definition and stable production are critical.

The material has a Shore A hardness of approximately 78, providing a relatively firm elastomeric response while maintaining very high elongation.

Current Celanese grade data lists approximately 460% elongation at break, 8.69 MPa stress at break and 3.76 MPa stress at 100% elongation.

The grade also offers approximately 27 kN/m tear strength, helping thin lips and complex profile sections resist tearing during processing, assembly and service.

Low-temperature performance is strong, with a brittleness temperature of approximately -60°C under both ASTM D746 and ISO 812-related testing.

For seals and profiles exposed to long-term compression, current Celanese data lists approximately 34% compression set at 70°C for 24 hours and 42% at 125°C for 70 hours.

Environmental resistance is a major part of the grade’s positioning. Celanese specifically describes excellent ozone resistance, excellent flex-fatigue resistance and improved UV resistance.

These characteristics are especially important in automotive exterior sealing, window and door profiles and weather-exposed elastomer components.

Santoprene 121-73W175 is UL recognized under Celanese file references QMFZ2.E80017 and QMFZ8.E80017. Current grade data lists UL 94 HB at 3.0 mm.

The material also has an electric strength of approximately 27 kV/mm at 2 mm, giving additional technical context for protective or electrically adjacent elastomeric components.

For more TPV products, visit our TPV Thermoplastic Vulcanizates Product Category →.

For the broader Celanese Santoprene portfolio, see the Official Celanese Santoprene & Geolast TPV Product Finder →.

Key Features of Santoprene 121-73W175

Feature Engineering Benefit
Shore A 78 Firmer elastomeric response for automotive sealing and profile applications
UV Resistant Designed for improved durability in sunlight and exterior service
Excellent Ozone Resistance Helps prevent cracking in weather-exposed applications
Excellent Flex-Fatigue Resistance Supports repeated movement and dynamic sealing
Thin-Wall Profile Capability Designed for fine profile definition down to approximately 0.33 mm radius
Reduced Extrusion Build-Up Supports longer runs with minimal material accumulation in narrow die sections
460% Elongation at Break High flexibility despite 78A hardness
8.69 MPa Stress at Break Strong mechanical performance for a flexible TPV
27 kN/m Tear Strength Useful for thin lips, profile edges and sealing details
-60°C Brittleness Temperature Supports cold-weather automotive applications
UL Recognized Current Celanese documentation references E80017
Thermoplastic Processing Compatible with conventional extrusion, thermoforming and vacuum-forming equipment
Polyolefin Based Low density and manufacturing-stream recyclability
Automotive OEM References Current grade data lists multiple global automotive specifications

Typical Applications for Santoprene 121-73W175

Santoprene 121-73W175 is particularly suited to complex and thin-section extruded components.

Application Area Typical Use
Automotive Weatherseals Exterior sealing profiles exposed to sunlight, ozone and temperature cycles
Glass Run Channels Flexible profile sections around automotive side glass
Door Sealing Profiles Complex extruded sealing geometries
Window Profiles Flexible UV-resistant sealing lips
Automotive Exterior Trim Elastomeric profile and sealing components
Automotive Interior Profiles Flexible trim and sealing sections
Under-Hood Profiles Flexible technical profiles with heat and ozone exposure
Thin-Wall Extrusions Fine-section profiles requiring precise definition
Complex Coextruded Profiles Soft TPV sealing section combined with compatible substrates
Electrical Protective Profiles Flexible UV-resistant protective components
Industrial Seals Continuous profiles requiring weatherability and flexibility

Celanese has also used Santoprene 121-73W175 as a benchmark material for glass run channel lip and foot applications, reinforcing its relevance to demanding automotive profile extrusion.

Typical Properties of Santoprene 121-73W175

Physical Properties

Property Typical Value Test Method
Density 970 kg/m³ / 0.970 g/cm³ ISO 1183
Shore A Hardness, 15 s 78 ISO 48-4 / ISO 868
Color Black Manufacturer information
Product Form Pellets Manufacturer information
Base Chemistry Polyolefin-based TPV Manufacturer information

Mechanical Properties

Property Typical Value Test Method
Stress at 100% Elongation 3.76 MPa ISO 527-1/-2 or ISO 37
Stress at Break 8.69 MPa ISO 527-1/-2 or ISO 37
Elongation at Break 460% ISO 527-1/-2 or ISO 37
Tear Strength, Normal 27 kN/m ISO 34-1
Brittleness Temperature -60°C ASTM D746
Low-Temperature Brittleness -60°C ISO 812
Compression Set, 70°C / 24 h 34% ISO 815
Compression Set, 125°C / 70 h 42% ISO 815

Aging Performance

Property Typical Change Test Condition
Tensile Strength Change -9% 150°C / 168 h
Elongation Change -2% 150°C / 168 h
Shore A Hardness Change +5 150°C / 168 h
Continuous Upper Temperature Resistance 135°C SAE J2236, 1008 h

Flammability & Electrical Properties

Property Typical Value Test Method
UL 94 Rating @ 3.0 mm HB UL 94
UL Recognition Yes UL 94
Electric Strength, 2 mm 27 kV/mm ASTM D149

Why Choose Santoprene 121-73W175?

The main reason to choose Santoprene 121-73W175 is the combination of profile-extrusion stability, UV resistance and elastomeric durability.

Extruding a complex automotive weatherseal is more demanding than molding a simple gasket. Thin sealing lips and narrow die sections can make melt stability, die build-up and edge definition critical to production efficiency.

Celanese specifically designed Santoprene 121-73W175 to address these challenges.

The grade can produce thin sections with fine definition, including geometry down to approximately 0.33 mm radius.

At the same time, it is intended to reduce material accumulation on screen packs and narrow die sections. This can support longer production runs and reduce interruptions for die cleaning.

The grade’s UV stabilization is another major advantage over standard black TPV grades that are not specifically optimized for outdoor profile exposure.

Excellent ozone resistance supports weatherseals and exterior components that may remain exposed to air, sunlight and fluctuating temperatures over many years.

Flex-fatigue resistance is important for door seals, glass-run-channel lips and dynamic sealing elements that bend every time a vehicle door or window operates.

The 460% elongation at break provides substantial deformation capability.

The 27 kN/m tear strength supports durability in thin edges and sealing lips.

For automotive profile manufacturers needing a black 78A TPV specifically tuned for thin-wall extrusion and long production runs, Santoprene 121-73W175 is more targeted than a basic general-purpose TPV.

Processing Guidelines for Santoprene 121-73W175

Santoprene 121-73W175 is primarily designed for extrusion and can also be processed by:

  • Profile extrusion
  • Coextrusion
  • Sheet extrusion
  • Thermoforming
  • Vacuum forming
  • Conventional thermoplastic extrusion equipment

Grade-Specific Extrusion Conditions

Processing Parameter Celanese Guidance
Drying Temperature 82°C
Drying Time 3 hours
Dryer Type Dehumidified / desiccant dryer
Melt Temperature Range 177–204°C
General Santoprene Processing Window 175–230°C
Maximum Drawdown 15%

Celanese recommends drying for approximately 3 hours at 80–82°C before processing.

For this grade, the published extrusion melt-temperature range is approximately 177–204°C.

The broader Santoprene family can be processed across approximately 175–230°C, but the grade-specific range should be the preferred starting point for production trials.

Drawdown Control

Celanese specifically states that drawdown should not exceed approximately 15%.

This is particularly important for thin-wall and complex extrusion profiles because excessive drawdown can change dimensions, wall thickness, lip geometry and surface quality.

Shear-Dependent Flow

Santoprene 121-73W175 is a shear-dependent TPV. As shear rate increases, apparent melt viscosity decreases.

Processors should optimize screw speed, melt temperature, screen-pack configuration, die pressure, die geometry, drawdown, cooling rate, haul-off speed and coextrusion balance.

Material Compatibility

Celanese states that Santoprene TPV is incompatible with acetal (POM) and PVC.

Extrusion lines should be properly purged when changing between these materials and Santoprene TPV.

Automotive OEM References for Santoprene 121-73W175

Current Celanese grade data lists numerous automotive references:

OEM / Organization Specification / Reference
Ford WSS-M2D280-B1
Ford WSS-M9P14-A1 / MCDCC JA6A
General Motors GMW15812 Type 6E
Mercedes-Benz Group DBL 5562
Hyundai MS220-05 Type P
MAN M3236 A7
Iveco IVECO 15-5244 EMP-70
Renault FRM 18-27-039 / –C
Stellantis / FCA 55248/02 EMP-70
Stellantis / Chrysler MS-AR-100 CGV
Volkswagen Group TL 526 41C
Volkswagen Group TL 527 03
Volkswagen Group VW50123
BAIC BAS-492
Geely Q/JLY J7110166B
SAIC Motor SMTC 5 320 024
Li Auto Q/LiA5310057
Bosch N28 BN34-OX 017

Santoprene 121-73W175 vs. Santoprene 121-67W175

Feature Santoprene 121-73W175 Santoprene 121-67W175
Material Family TPV TPV
Color Black Black
Main Positioning UV profile extrusion UV profile extrusion
Shore A Hardness 78 72
Elongation at Break 460% 432%
Tensile Stress at Break 8.7 MPa 6.8 MPa
Stress @ 100% Elongation 3.8 MPa 2.9 MPa
Compression Set, 70°C 34% 29%
UV Stability Yes Yes
Profile Extrusion Tuning Yes Yes
Main Selection Difference Firmer, stronger profile Softer, more compliant profile

Choose Santoprene 121-73W175 when greater hardness and tensile strength are required in a UV-resistant extrusion profile.

Choose Santoprene 121-67W175 when the design requires a softer and more compliant profile.

Related Products

Santoprene 121-67W175 – Softer UV-resistant black TPV tuned for profile extrusion, approximately Shore A 72.

Santoprene 121-58W175 – Softer profile-extrusion TPV with approximately Shore A 61 hardness.

Santoprene 121-80W175 – Firmer UV-stabilized W175 profile-extrusion grade with approximately Shore A 85 hardness.

View More TPV Thermoplastic Vulcanizates →

Technical Documents for Santoprene 121-73W175

Document Type Description
TDS Current Celanese physical, mechanical and extrusion data
SDS Safety Data Sheet
UL Information QMFZ2.E80017 / QMFZ8.E80017 recognition
Automotive Specification Information Ford, GM, Mercedes-Benz, Hyundai, VW and other OEM references
Santoprene Product Finder Current Celanese grade comparison and application positioning
Processing Guide Extrusion and profile-processing guidance
COA Batch-specific quality information where available

Need technical documents for Santoprene 121-73W175?

📧 Email: ruiqingchem@gmail.com
📝 Online form: Contact Us →

Please state Santoprene 121-73W175 and the required document type when submitting your inquiry.

FAQ About Santoprene 121-73W175

Q1: What is Santoprene 121-73W175?

Santoprene 121-73W175 is a black UV-resistant TPV from Celanese designed for thin-wall and complex profile extrusion.

Q2: What is the hardness of Santoprene 121-73W175?

The current Shore A hardness is approximately 78.

Q3: What is the tensile stress at break?

Current Celanese grade data lists approximately 8.69 MPa.

Q4: What is the elongation at break?

The current elongation at break is approximately 460%.

Q5: Is Santoprene 121-73W175 UV resistant?

Yes. Celanese specifically describes the grade as designed for improved UV resistance and includes it in the UV-black TPV family.

Q6: Is Santoprene 121-73W175 suitable for thin-wall profile extrusion?

Yes. Celanese specifically designed the grade for thin-wall and complex profiles, including fine geometry down to approximately 0.33 mm radius.

Q7: What is the low-temperature performance?

The current brittleness temperature is approximately -60°C.

Q8: What extrusion temperature is recommended?

The grade-specific published melt-temperature range is approximately 177–204°C.

Q9: What is the maximum recommended drawdown?

Celanese states that drawdown should not exceed approximately 15%.

Q10: What is the difference between Santoprene 121-73W175 and 121-67W175?

Both are UV-resistant black W175 grades tuned for profile extrusion. 121-73W175 is harder at Shore A 78 and has higher tensile strength, while 121-67W175 is softer at approximately Shore A 72.

Request Santoprene 121-73W175 Price & Technical Support

For pricing, availability, technical documents or application support for Santoprene 121-73W175, please provide:

  • Required quantity
  • Destination country or port
  • Automotive or industrial application
  • Weatherseal, glass-run-channel or other profile design
  • Required Shore hardness
  • Profile wall thickness
  • Minimum lip or corner radius
  • UV and outdoor exposure
  • Service temperature range
  • Compression-set requirement
  • Extrusion line and screw configuration
  • Coextrusion requirement
  • OEM specification requirement
  • TDS, SDS, UL or COA requirement
  • Sample requirement, if applicable

📧 Email: ruiqingchem@gmail.com
📝 Send Inquiry →

Technical Documents

Download technical data sheets, safety data sheets and certificates for this material.

TDS Files

Technical document available for review or download.

0 Files
No TDS file uploaded yet.

MSDS Files

Technical document available for review or download.

0 Files
No MSDS file uploaded yet.